PENELITIAN UJI KUAT TEKAN BETON DENGAN MEMANFAATKAN LIMBAH AMPAS TEBU DAN ZAT ADDITIF SIKACIM BONDING ADHESIVE

Authors

  • Agil Dwi Krisna Fakultas Teknik Universitas Kadiri
  • Sigit Winarto Fakultas Teknik Universitas Kadiri
  • Ahmad Ridwan Fakultas Teknik Universitas Kadiri

DOI:

https://doi.org/10.30737/jurmateks.v2i1.385

Keywords:

Compressive Strength, Bagasse, Additive, Concrete

Abstract

Concrete has the disadvantage of having a low tensile strength and convincing brittle beams with steel inscriptions to anticipate. In this study, the concrete mixture was given additional bagasse and additives of cycacim bonding. This addition was carried out to study and study the effect of bagasse on the compressive strength of normal k300 concrete by replacing bagasse by 0%, 5%, 10% and 15% in compressive loads. Compressive strength specimens in the form of cubes with a size of 15 cm x 15 cm x 15 cm. Testing is done after 28 days. Concrete with increased bagasse of 5% is better able to produce high compressive strength values than others. The addition of bagasse resulted in an average compressive strength of 5%, 229.64 kg / cm2, 10%, 190.35 kg / cm2, 15%, 160.87 kg / cm2.

Beton mempunyai kelemahan yaitu mempunyai kuat tarik yang rendah dan bersifat getas sehingga beton diberi tulangan baja untuk mengantisipasinya. Pada penelitian ini, campuran beton diberi bahan tambahan ampas tebu dan zat additif sikacim bonding adhesive. Penambahan ini dilakukan untuk mempelajari dan mengetahui pengaruh ampas tebu terhadap kuat tekan pada beton mutu normal k300 dengan penambahan ampas tebu sebesar 0%, 5%, 10% dan 15% pada beban tekan. Benda uji kuat tekan berbentuk kubus dengan ukuran 15 cm x 15 cm x 15 cm. Pengujian dilakukan setelah 28 hari. Beton dengan penambahan ampas tebu 5% lebih mampu menghasilkan nilai kuat tekan tinggi dari pada yang lainya. Penambahan ampas tebu menghasilakan kuat tekan rata-rata yaitu 5%,229,64 kg/cm2, 10%,190,35 kg/cm2, 15%,160,87kg/cm2.


References

T. Mulyono, “TEKNOLOGI BETON: Dari Teori Ke Praktek,†no. October 2018, p. 574, 2015.

A. Y. Bintoro, A. D. Limantara, and S. Winarto, “EVALUASI KEKUATAN CONCBLOCK DENGAN AGREGAT HALUS DAN AGREGAT KASAR DARI TEMPURUNG KELAPA,†Jurmateks, vol. 1, no. 1, pp. 160–171, 2018.

D. U. Sudarsono, “Rencana Campuran (Mix Design),†p. 1993, 1993.

E. Siswanto and A. Gunarto, “PENAMBAHAN FLY ASH DAN SERAT SERABUT KELAPA,†Ukarst J. Univ. Kadiri Ris. Tek. Sipil, vol. 3, no. 1, pp. 56–65, 2019.

M. M. Amin, A. D. Limantara, and S. Winarto, “UJI LABORATORIUM PEMANFAATAN BIO ENZIM (BIOCONC) SEBAGAI PEREDUKSI SEMEN PADA BATA BETON MUTU A,†Jurmateks, vol. 1, no. 1, pp. 56–65, 2018.

SNI 2847:2013, “Persyaratan beton struktural untuk bangunan gedung,†Badan Stand. Nas., 2013.

E. Gardjito, A. I. Candra, and Y. Cahyo, “Pengaruh Penambahan Batu Karang Sebagai Substitusi Agregat Halus Dalampembuatan Paving Block,†UKaRsT, vol. 2, no. 1, p. 35, 2018, doi: 10.30737/ukarst.v2i1.374.

A. D. Limantara, A. Widodo, S. Winarto, L. D. Krisnawati, and S. W. Mudjanarko, “Optimizing the use of natural gravel Brantas river as normal concrete mixed with quality fc = 19.3 Mpa,†IOP Conf. Ser. Earth Environ. Sci., vol. 140, no. 1, pp. 1–9, 2018, doi: 10.1088/1755-1315/140/1/012104.

JIS A 1148:2010, “Method of Test for Resistance of Concrete to Freeze and Thawing.†.

R. B. Anugraha and S. Mustaza, “Beton Ringan dari Campuran Styrofoam dan Serbuk Gergaji dengan Semen Portland 250, 300 dan 350 kg/m3,†J. Apl. Tek. Sipil, vol. 8, no. 2, p. 57, 2010, doi: 10.12962/j12345678.v8i2.2722.

A. Iwan and E. Siswanto, “MENGGUNAKAN HYDROTON DAN MASTER EASE 5010,†J. CIVILLa, vol. 3, no. 2, pp. 162–165, 2018.

Badan Standardisasi Nasional, “Tata Cara Perhitungan Struktur Beton Untuk Bangunan Gedung. SNI 03-2847-2002,†Bandung Badan Stand. Nas., p. 251, 2002.

A. I. Candra, E. Gardjito, Y. Cahyo, and G. A. Prasetyo, “Pemanfaatan Limbah Puntung Rokok Filter Sebagai Bahan Campuran Beton Ringan Berpori,†UKaRsT, vol. 3, no. 1, p. 82, 2019, doi: 10.30737/ukarst.v3i1.365.

A. I. Candra and E. Siswanto, “Rekayasa Job Mix Beton Ringan Menggunakan Hydroton Dan Master Ease 5010,†J. CIVILA, vol. 3, no. 2, p. 162, 2018, doi: 10.30736/cvl.v3i2.258.

SNI 2493:2011, “Tata cara pembuatan dan perawatan benda uji beton di laboratorium,†Badan Stand. Nas., 2011.

R. Manuahe et al., “Kuat Tekan Beton Geopolymer Berbahan Dasar Abu Terbang,†J. Sipil Statik, vol. 2, no. 1, pp. 277–282, 2014, doi: 10.5614/jts.2013.20.1.1.

SNI 3402:2008, “Cara uji berat isi beton ringan struktural,†Badan Stand. Nas., 2008.

A. C. Sembiring and J. J. Saruksuk, “Uji Kuat Tekan Dan Serapan Air Pada Paving Block dengan Bahan Pasir Kasar, Batu Kacang, dn Pasir Halus,†JURITI PRIMA (Junal Ilm. Tek. Ind. Prima), vol. 1, no. May, 2018, doi: 10.5281/zenodo.1207331.

M. Mulyati and A. Adman, “Pengaruh Penambahan Cangkang Kemiri dan Sikacim Concrete Additive terhadap Kuat Tekan Beton Normal,†J. Tek. Sipil ITP, vol. 6, no. 2, pp. 38–45, 2019, doi: 10.21063/jts.2019.v602.01.

SNI 1974:2011, “Cara uji kuat tekan beton dengan benda uji silinder,†Badan Stand. Nas., 2011.

T. P. G. A, Y. C. S. P, S. Winarto, and A. I. Candra, “PERBANDINGAN KEKUATAN BETON DENGAN CAMPURAN DRAMIX STEEL FIBER DAN TULANGAN WIREMESH PADA RIGID PAVEMENT,†Jurmateks, vol. 1, no. 2, pp. 313–324, 2018.

D. Hartanto, Y. Cahyo, S. Winarto, and A. I. Candra, “PERENCANAAN PONDASI TIANG PANCANG PADA GEDUNG SEKRETARIAT DEWAN DPRD KABUPATEN KEDIRI,†Jurmateks, vol. 1, no. 2, pp. 303–312, 2018.

Downloads

PlumX Metrics

Published

2019-05-25

Issue

Section

Articles