Penelitian Beton dengan Penambahan Abu Sekam Padi dan Limbah Keramik sebagai Substitusi Semen

Authors

  • Olyndia Febrianita Fakultas Teknik, Universitas Kadiri
  • Ahmad Ridwan Fakultas Teknik, Universitas Kadiri
  • Yosef Cahyo Setianto Poernomo Fakultas Teknik, Universitas Kadiri

DOI:

https://doi.org/10.30737/jurmateks.v3i2.1138

Keywords:

Cement Substitution, Ceramic Waste, Lightweight Concrete, Rice Husk Ash

Abstract

Concrete is a technology that continues to develop in the construction sector. Continues to increase in terms of cost. The need for materials to form concrete requires innovation in the use of concrete mixtures. One of them is using the innovation of rice husk ash and ceramic waste. These ingredients is held in the cement content, namely rice husk ash containing silica and ceramic waste containing alumina. The method used refers to the Indonesian National Standard with a cylindrical specimen measuring 15x30 cm tested at 28 days, and the planned quality is fc '14.5 Mpa. The research objective was to determine the compressive strength and slump value by adding a mixture of rice husk ash 3%, 6%, 9%, 12%, and ceramic waste 3% by weight of cement. The results showed that the slump value decreased with the lowest value of 13.5 cm. the results of the compressive strength of concrete with the addition of rice husk ash and ceramic waste have not achieved the planned quality. The average compressive strength that has the highest value is the addition of 9% rice husk ash with 9% ceramic waste, namely 6.53 Mpa.

Beton merupakan salah satu teknologi yang terus berkembang di bidang konstruksi. Terus meningkat dari segi biaya, Kebutuhan bahan untuk membentuk beton membutuhkan inovasi dalam penggunaan campuran beton. Salah satunya dengan inovasi pemanfaatan abu sekam padi dan limbah keramik. Bahan tersebut tertahan di dalam kandungan semen yaitu abu sekam padi yang mengandung silika dan limbah keramik yang mengandung alumina. Metode yang digunakan mengacu pada Standar Nasional Indonesia dengan spesimen silinder berukuran 15x30 cm yang diuji pada 28 hari, dan kualitas yang direncanakan adalah fc '14 .5 Mpa. Tujuan penelitian untuk mengetahui kuat tekan dan nilai slump dengan menambahkan campuran abu sekam padi 3%, 6%, 9%, 12%,   dan   limbah   keramik   3%   dari   berat  semen.   Hasil Penelitian menunjukkan nilai slump mengalami penurunan dengan nilai terendah 13,5cm. Hasil kuat tekan beton dengan penambahan abu sekam padi dan limbah keramik belum mencapai kualitas yang direncanakan. Kuat tekan rata-rata yang memiliki nilai tertinggi adalah penambahan abu sekam 9% dengan limbah keramik 9% yaitu 6,53 Mpa

References

Y. Cahyo and R. Ajiono, “ANALISA JOBMIX NILAI MUTU BATU BATA DENGAN MENGGUNAKAN LIMBAH ABU SERAT TEBU DAN ABU SERBUK GERGAJI,†UkaRsT, vol. 1, no. 1, pp. 55–63, 2017.

R. Hepiyanto and D. Kartikasari, “PENGARUH CAMPURAN AIR LIMBAH (AIR SELOKAN) TERHADAP KUAT TEKAN BETON f’c 14.5 Mpa (K-175),†UkaRsT, vol. 2, no. 2, 2018.

Revisdah and R. Utari, “PEMANFAATAN LIMBAH KERAMIK TERHADAP KUAT TEKAN BETON,†Pros. Semnastek, 2018.

F. S. Ridwan, “ANALISIS PENGARUH PEMANFAATAN ABU SEKAM SEBAGAI FILLER PADA CAMPURAN ASPAL BETON,†Konstruksia, vol. 8, no. 2, pp. 1–8, 2017.

S. H. Kang, S. G. Hong, and J. Moon, “The use of rice husk ash as reactive filler in ultra-high performance concrete,†Cem. Concr. Res., vol. 115, no. March, pp. 389–400, 2019, doi: 10.1016/j.cemconres.2018.09.004.

A. S. Huda and Suprapto, “Pengaruh Limbah Keramik Sebagai Pengganti Agregat Halus Terhadap Mutu Beton,†J. Kaji. Pendidik. Tek. Bangunan, vol. 3, no. 1, 2013.

D. M. Kannan, S. H. Aboubakr, A. S. EL-Dieb, and M. M. Reda Taha, “High performance concrete incorporating ceramic waste powder as large partial replacement of Portland cement,†Constr. Build. Mater., vol. 144, pp. 35–41, 2017, doi: 10.1016/j.conbuildmat.2017.03.115.

A. Ridwan, S. Winarko, and E. Siswanto, “Jobmix beton mengunakan pasir lumajang dan penambahan additive masterpozzolith ® 402R,†J. CIVILLa, vol. 3, no. 2, pp. 192–197, 2018.

S. Raharja, S. As’ad, and Sunarmasto, “Pengaruh Penggunaan Abu Sekam Padi Sebagai Bahan Pengganti Sebagian Semen Terhadap Kuat Tekan Dan Modulus Elastisitas Beton Kinerja Tinggi,†e-Jurnal Matriks Tek. Sipil, vol. 1, no. 4, pp. 503–510, 2013.

M. A. Anshori, A. Ridwan, and Y. C. SP, “PENELITIAN UJI KUAT TEKAN BETON DENGAN MEMANFAATKAN AIR LIMBAH TETES TEBU DAN ZAT ADDITIVE CONCRETE,†Jurmateks, vol. 2, no. 1, pp. 16–28, 2019.

M. Aslam, P. Shafigh, M. Z. Jumaat, and M. Lachemi, “Benefits of using blended waste coarse lightweight aggregates in structural lightweight aggregate concrete,†J.Clean. Prod., vol. 119, pp. 108–117, 2016, doi: 10.1016/j.jclepro.2016.01.071.

M. M. Al Bakri Abdullah, K. Hussin, M. Bnhussain, K. N. Ismail, Z. Yahya, and R. A. Razak, “Fly ash-based geopolymer lightweight concrete using foaming agent,†Int. J. Mol. Sci., vol. 13, no. 6, pp. 7186–7198, 2012, doi: 10.3390/ijms13067186.

S. Puro, “KAJIAN KUAT TEKAN DAN KUAT TARIK BETON RINGAN MEMANFAATKAN SEKAM PADI DAN FLY ASH DENGAN KANDUNGAN SEMEN 350 kg/m3,†J. Ilm. Media Eng., vol. 4, no. 2, p. 97931, 2014.

E. Siswanto and A. Gunarto, “PENAMBAHAN FLY ASH DAN SERAT SERABUT KELAPA SEBAGAI BAHAN PEMBUATAN BETON,†UKaRsT, vol. 3, no. 1, pp. 56–65, 2019.

M. S. Nadesan and P. Dinakar, “Mix design and properties of fly ash waste lightweight aggregates in structural lightweight concrete,†Case Stud. Constr. Mater., vol. 7, no. May, pp. 336–347, 2017, doi: 10.1016/j.cscm.2017.09.005.

S. Winarto, “Pemanfaatan Serat Ijuk Sebagai Material Campuran Dalam Beton Untuk Meningkatkan Kemampuan Beton Menahan Beban Tekan Studi Kasus: Pembangunan Homestay Singonegaran Kediri,†UKaRsT, vol. 1, no. 1, pp. 1–10, 2017.

E. Hunggurami, M. E. Bolla, and P. Messakh, “PERBANDINGAN DESAIN CAMPURAN BETON NORMAL MENGGUNAKAN SNI 03-2834-2000 DAN SNI 7656:2012,†Tek. Sipil, vol. VI, no. 2, pp. 165–172, 2017.

A. I. Candra, E. Gardjito, Y. Cahyo, and G. A. Prasetyo, “Pemanfaatan Limbah Puntung Rokok Filter Sebagai Bahan Campuran Beton Ringan Berpori,†UKaRsT, vol. 3, no. 1, p. 82, 2019, doi: 10.30737/ukarst.v3i1.365.

Y. Sandya and S. Musalamah, “PENGGUNAAN ABU SEKAM PADI SEBAGAI PENGGANTI SEMEN PADA BETON GEOPOLIMER,†Educ. Build. J. Pendidik. Tek. Bangunan dan Sipil, vol. 5, no. 2, pp. 59–63, 2019.

H. Chao-Lung, B. Le Anh-Tuan, and C. Chun-Tsun, “Effect of rice husk ash on the strength and durability characteristics of concrete,†Constr. Build. Mater., vol. 25, no. 9, pp. 3768–3772, 2011, doi: 10.1016/j.conbuildmat.2011.04.009.

M. I. Saifuddin, B. Edison, and K. Fahmi, “Pengaruh Penambahan Campuran Serbuk Kayu Terdahap Kuat Tekan Beton,†J. Mhs. Tek., vol. 1, no. 1, 2013.

S. 1974:2011, “SNI 1974:2011 tentang Cara Uji Kuat Tekan Beton dengan Benda Uji Silinder,†Badan Stand. Nas., p. 20, 2011.

Downloads

PlumX Metrics

Published

2020-10-30

Issue

Section

Articles