UJI KUAT TEKAN DAN ARBSORPSI PADA BETON RINGAN DENGAN PENAMBAHAN LIMBAH BATA RINGAN DAN BUBUK TALEK

Authors

  • Krisna Dwi Kurniawan Fakultas Teknik Universitas Kadiri
  • Ahmad Ridwan Fakultas Teknik Universitas Kadiri
  • Yosef Cahyo Fakultas Teknik Universitas Kadiri

DOI:

https://doi.org/10.30737/jurmateks.v3i1.872

Keywords:

Compressive Strength, Lightweight Brick, Lightweight Concrete, Talek Powder

Abstract

Concrete is one of the construction components used in buildings, bridges, or roads. In this study, The authors learned to create concrete that is lighter than standard concrete, that is by using light cement with a weight of 0%, 10% 20%, 30%, 40% of the volume of sand and talc powder weighing 8% of the volume of cement. The strength targeted in this study is k-225. Meanwhile, this study's results are the value of concrete compressive strength, which is increased by the target set k-225 to be k-400 in one of the normal concrete samples and has an average of k-360. 10% 20%, 30%, 40% and 8% talc powder increase with each average yield of k-294, k271, k-251, and k-225. To check the absorption of concrete samples, check the average increase in immersion 1 hour 0.0016%, 4 hours 0.0027%, and 24 hours 0.0047%. For the results of testing the type of weight, from each variation of test specimens 1 - 5, the resolution decreases 2.26, 2.24, 2.23, 2.16, and 2.028. The one with the lowest specific gravity is variation five concrete, with a variation of the average specific gravity 2,028.


Beton merupakan salah satu komponen konstruksi yang pada umumnya digunakan pada bangunan gedung, jembatan maupun jalan. Pada penelitian ini Penulis bertujuan untuk menciptakan Beton yang lebih ringan dari pada Beton normal yaitu  menggunakan tambahan limbah bata ringan dengan bobot 0% , 10% 20%, 30%, 40% dari volume pasir dan bubuk talek dengan bobot 8% dari volume semen. Kekuatan yang ditargetkan pada penelitian ini adalah k-225. Adapun hasil dari penelitian ini adalah nilai kuat tekan Beton mengalami peningkatan target yaitu yang awalnya k-225 menjadi k-400 pada salah satu sampel Beton normal dan memiliki rata- rata k-360. Kemudian hasil nilai kuat tekan Beton dengan penambahan limbah bata ringan  10% 20%, 30%, 40% dan bubuk talek 8% mengalami penurunan yaitu dengan masing-masing hasil rata- rata k-294, k271,k-251, dan k-225. Untuk pemeriksaan arbsorpsi Beton sampel mengalami kenaikaan rata-rata yaitu pada perendaman 1 Jam 0,0016%, 4 Jam 0,0027% dan 24 Jam 0,0047%. Untuk hasil pemeriksaan berat jenis, dari setiap benda uji dari variasi 1 – 5 mengalami penurunan masing masing 2,26, 2,24, 2,23, 2,16 dan 2,028 maka yang memiliki berat jenis paling rendah adalah Beton variasi 5 yaitu dengan rata rata berat jenis 2,028.


References

A. I. Candra, H. Wahyudiono, S. Anam, and D. Aprillia, “KUAT TEKAN BETON Fc ’ 21 , 7 MPa MENGGUNAKAN WATER REDUCING AND HIGH RANGE ADMIXTURES,†vol. 5, no. 1, 2020.

Zulkifly, N. H. Aswad, and R. Talanipa, “Pengaruh Penambahan Serat Sabut Kelapa Terhadap Kuat Tekan Beton pada Beton Normal,†Stabilita, vol. 1, no. 2, pp. 121–128, 2013.

S. Handayani, “Analisis Pengujian Struktur Balok Laminasi Kayu Sengon Dan Kayu Kelapa,†J. Tek. Sipil dan Perenc., vol. 18, no. 1, pp. 39–46, 2016, doi: 10.15294/jtsp.v18i1.6693.

H. Suseno, Bahan Bangunan Untuk Teknik Sipil. Malang: Bargie Media, 2010.

C.-K. Wang and C. G. Salmon, Disain Beton Bertulang. Jakarta: Erlangga, 1986.

R. B. Anugraha and S. Mustaza, “Beton Ringan dari Campuran Styrofoam dan Serbuk Gergaji dengan Semen Portland 250, 300 dan 350 kg/m3,†J. Apl. Tek. Sipil, vol. 8, no. 2, p. 57, 2010, doi: 10.12962/j12345678.v8i2.2722.

A. I. Candra, E. Gardjito, Y. Cahyo, and G. A. Prasetyo, “Pemanfaatan Limbah Puntung Rokok Filter Sebagai Bahan Campuran Beton Ringan Berpori,†UKaRsT, vol. 3, no. 1, p. 82, 2019, doi: 10.30737/ukarst.v3i1.365.

F. octaviani Lomboan, ellen j. Kummat, and R. S. Windah, “Pengujian Kuat Tekan Mortar Dan Beton Ringan Dengan Menggunakan Agregat Ringan Batu Apung Dan Abu Sekam Padi Sebagai Substitusi Parsial Semen,†J. Sipil Statik, vol. 4, no. 4, pp. 271–278, 2016.

A. Syarif, C. Setyawan, and I. Farida, “Analisa Uji Kuat Tekan Beton Dengan Bahan Tambahan Batu Bata Merah,†J. STT-Garut, vol. 14, no. 1, pp. 46–56, 2016.

Badan Standarisasi Nasional, Tata Cara Perhitungan Struktur Beton Untuk Bangunan Gedung. Bandung: Badan Standarisasi Nasional, 2002.

A. D. Krisna, S. Winarto, and A. Ridwan, “MEMANFAATKAN LIMBAH AMPAS TEBU DAN ZAT ADDITIF SIKACIM BONDING ADHESIVE,†Jurmateks, vol. 2, no. 1, pp. 1–15, 2019.

A. Asroni, Balok dan Pelat Beton Bertulang. Yogyakarta: Graha Ilmu, 2010.

PBI 1971 N.I. - 2, “Peraturan Beton Bertulang indonesia 1971 N.I. - 2,†Jakarta Direktorat Penyelid. Masal. Bangunan, vol. 7, p. 130, 1971.

M. A. Anshori, A. Ridwan, and Y. C. SP, “PENELITIAN UJI KUAT TEKAN BETON DENGAN MEMANFAATKAN AIR LIMBAH TETES TEBU DAN ZAT ADDITIVE CONCRETE,†Jurmateks, vol. 2, no. 1, pp. 16–28, 2019.

Tjokrodimuljo, “Material Penyusun Beton,†J. Swidodo Tek. Sipil Univ. Negeri Yogyakarta, pp. 1–23, 1996.

E. Gardjito, A. I. Candra, and Y. Cahyo, “Pengaruh Penambahan Batu Karang Sebagai Substitusi Agregat Halus Dalam Pembuatan Paving Block,†UKaRsT, vol. 2, no. 1, p. 35, 2018, doi: 10.30737/ukarst.v2i1.374.

K. Tjokrodimuljo, “Teknologi Beton,†Biro Penerbit Tek. Sipil Univ. Gajah Mada, 2009.

Z. Zainuri, G. Yanti, and S. W. Megasari, “Optimasi Metode Pemisahan Serat Pelepah Kelapa Sawit Terhadap Kuat Tekan Bata Ringan,†SIKLUS J. Tek. Sipil, vol. 4, no. 2, pp. 80–90, 2018, doi: 10.31849/siklus.v4i2.1186.

E. Doe, “Perencanaan Kombinasi Beton dengan Metode Departement of Environment ( DoE),†vol. 4, no. November, pp. 602–612, 2019.

S. Winarto, “Pemanfaatan Serat Ijuk Sebagai Material Campuran Dalam Beton Untuk Meningkatkan Kemampuan Beton Menahan Beban Tekan Studi Kasus: Pembangunan Homestay Singonegaran Kediri,†UKaRsT, vol. 1, no. 1, pp. 1–10, 2017.

M. Sumajouw, S. Dapas, and R. Windah, “Pengujian Kuat Tekan Beton Mutu Tinggi,†J. Ilm. Media Eng., vol. 4, no. 4, p. 97267, 2014.

E. Siswanto and A. Gunarto, “PENAMBAHAN FLY ASH DAN SERAT SERABUT KELAPA SEBAGAI BAHAN PEMBUATAN BETON,†UKaRsT, vol. 3, no. 1, pp. 56–65, 2019.